Bonding and debonding compound semiconductor wafers
Compound semiconductor wafers are some of the most valuable substrates in any fab, and some of the most fragile. Indium phosphide and gallium arsenide are brittle and soft, they’re often thin to begin with, and they expand with heat at a different rate from most carriers. Temporary bonding works well on them, but every step needs a little more care than it would with silicon.
Thermal expansion mismatch
When a bonded pair is heated or cooled, each wafer expands or shrinks at its own rate. If the rates differ, the pair bows and the bond line carries stress, which can crack a thin, brittle wafer during cooling or debonding.
| Material | Thermal expansion (ppm/K, approximate) |
|---|---|
| Silicon | 2.6 |
| Fused silica | 0.55 |
| Borosilicate glass | 3.25 |
| Indium phosphide | 4.6 |
| Gallium arsenide | 5.7 to 6.9 |
| Sapphire | 7.0 to 7.7 |
Choosing a carrier with an expansion close to the device wafer, and keeping temperature changes slow, keeps that stress low. Glass carriers can be chosen to suit, and sapphire suits some compound semiconductors.
Brittle and soft
Indium phosphide is especially delicate. It’s soft and brittle, with a much lower stiffness than silicon, so it chips at the edge, cracks under point loads and scratches easily. Thin wafers should be supported across their whole face on porous chucks, handled as little as possible and never clamped hard at the edge.
Gentle heating and cooling
Thermal shock is the main risk. Bring the bonded pair up to temperature and back down gradually.
- On a hotplate, proximity baking and programmable lift pins lower the wafer towards the plate in steps, so it warms gently. Our bake methods guide explains how.
- In the bonder and debonder, use controlled ramps and let the pair cool before handling.
A worked example
In one CEE process, 100 mm indium phosphide wafers were bonded to 150 mm sapphire carriers at 130°C, with 2,000 N of force for 180 seconds under vacuum at about 0.5 kPa. The bonded wafers reached a TTV below 5% and were thinned to 100 µm. They were then debonded on a thermal slide debonder at 190°C, at about six minutes a wafer, and all five wafers in the trial came off intact. The adhesive was cleaned off by spray on an Apogee spin developer.
Debonding
A thermal slide debond works well when the adhesive softens at a temperature the devices tolerate, with a slow, controlled slide. Mechanical peel from a release layer avoids reheating altogether. Whichever method you use, support the thin wafer across its whole face and move it as little as possible. Our guide to debonding methods compares the options.
How SiSTEM can help
CEE’s temporary bonding and debonding tools, the Apogee Temporary Bonder, the Apogee Thermal Slide Debonder and the Mechanical Debonder, have been qualified with indium phosphide, gallium arsenide, gallium nitride, silicon carbide, sapphire, silicon and glass wafers. Tell us your wafers, carrier and process temperatures, and we’ll work through the process with CEE’s applications team.