Temporary bonding adhesives and carriers

A temporary bond has to do two jobs that pull in opposite directions. It must hold a thin wafer firmly through grinding, etching, high temperature and harsh chemistry, and then let go cleanly at the end. The adhesive and the carrier are chosen together, around the hottest step in the process and the debond method you plan to use.

Adhesive types

  • Thermoplastic adhesives soften when heated, so they can be debonded by heating and sliding the wafers apart. Many flow at around 200°C, which also limits the process temperature they can survive. They’re simple to use and easy to clean off.
  • Curable adhesives cross-link during bonding and stand up to higher temperatures and harsher chemistry, but they don’t soften again, so they need a release layer and a mechanical, laser or solvent debond.
  • Waxes are the oldest option and still useful for low-temperature work and small batches.

Organic adhesives in general top out below about 300°C. Suppliers group their materials by temperature, for example up to about 225°C, up to about 350°C and above 350°C, so match the class to the hottest step in your flow, with a margin.

What to ask of an adhesive

  • Temperature: the highest process temperature it survives without flowing, outgassing or decomposing.
  • Chemistry: resistance to the solvents, acids and developers in the backside process.
  • Thickness and flatness: enough to cover the device topography, and uniform enough to keep total thickness variation (TTV) low. A common target is below about 5% of the adhesive thickness, or around 2 µm.
  • Release: compatible with the debond method, and easy to clean without damaging the device.

Carriers

CarrierWhy it’s used
SiliconCheap, flat, familiar to every fab tool, same thermal expansion as silicon device wafers
GlassTransparent, so needed for UV or laser release; expansion can be matched to the device wafer
SapphireRigid and chemically tough; closer in expansion to some compound semiconductors

Carriers are usually cleaned and reused. Thermal expansion matters most when the device wafer isn’t silicon, which our guide to bonding compound semiconductor wafers covers.

Avoiding voids

Voids are pockets of trapped air or solvent between the wafers. They leave the thin wafer unsupported, so it thins unevenly, chips or cracks during grinding. To avoid them:

  1. Coat evenly and check the adhesive film before bonding.
  2. Bake out the solvent in stages, typically somewhere between about 120 and 180°C, so it can’t gas out under the bond.
  3. Bond under vacuum, typically well below 5 mTorr, so no air is trapped.
  4. Apply even pressure and heat, then cool slowly to avoid stress.

How SiSTEM can help

The CEE Apogee Temporary Bonder bonds wafers from 2″ to 300 mm under vacuum, at up to 300°C and with 550 to 12,000 N of bond force, and Apogee spin coaters and bake plates prepare the adhesive layer. Our temporary bond and debond page covers the full set of tools. Tell us your adhesive, carrier and process temperatures, and we’ll set up a starting recipe with CEE.

More technical guides

All technical guides